I've learned more in the past few months than I ever did back when I was 16 and trying to build Guillows models and one trick I've started using is to pre-shrink tissue. I have a few question on the subject for you more experienced builders:
1) How do you shrink your tissue? I hijacked a picture frame from my wife and I cut off pieces of tissue about 10"x8" and glue them with a glue stick to the frame and shrink them with 50:50 isopropanol:water. This works well for 500 and 900 series size models but won't work well when I want to do something bigger. I only use the pre-shrunk stuff on tail surfaces and wings.
2) How much does pre-shrunk tissue shrink after you've covered the framework? I'm wondering because I thought I had a model pretty well covered but after doping it stretched more than I thought it would. (Aerogloss dope) I used Krylon on a model and didn't like the finish.
Any info or suggestions are always appreciated.